3M 471
Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

Main features
- Conformable Irregular-Surface Marking
- Clean-Removal Paint Masking
- Vivid Abrasion-Resistant Identification
Product Description
3M Vinyl Tape 471 is a conformable colored vinyl tape with rubber adhesive for lane and safety marking, color coding, paint masking, sealing, and temporary surface protection. The 0.14 mm tape stretches around curved, convex, and irregular surfaces while retaining its applied shape. Pigmented backings maintain vivid color under heavy abrasion, and the tape removes cleanly from many surfaces. Good solvent resistance and a choice of seven colors support plant marking and general process use. Apply the tape to clean, dry surfaces at 16 to 27 deg C for best results.
Key features
- Conformable dead stretch: The vinyl backing follows curved and irregular surfaces without lifting or retracting.
- Clean surface removal: Rubber adhesive provides immediate holding strength and clean removal from many surfaces.
- Abrasion-resistant color: Pigmented backings retain vivid identification colors under heavy abrasion.
Applications
Applications include lane and safety marking, color coding, fine-line paint masking, temporary surface protection, container sealing, bundling, and decorating.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Other Properties
Mechanical Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Color | Yellow, white, red, black, green, orange, blue | Pigmented backing | |
| Adhesive type | Rubber | Pressure-sensitive | |
| Backing thickness | 0.1 | mm | ASTM D3652; typical |
| Total tape thickness | 0.14 | mm | ASTM D3652; typical |
| Shelf life | 18 | months | Original packaging; 16 to 27 deg C and 40 to 60% RH; out of direct sunlight |
After-processing / final-state properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| 180 deg peel adhesion | 2.5 | N/cm | ASTM D3330; 23 deg C; 300 mm/min; typical |
| Elongation at break | 130 | % | ASTM D3759; typical |
| Tensile strength | 24.5 | N/cm | ASTM D3759; typical |
| Long-term temperature resistance | 77 | deg C | Days to weeks; typical |
| Minimum long-term temperature resistance | 4 | deg C | Days to weeks; typical |