3M 69
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Main features
- High-Temperature Electrical Insulation
- Glass-Cloth Coil and Motor Wrapping
- No-Heat Adhesive Application
Product Description
3M Glass Cloth Electrical Tape 69 is a white, 0.178 mm electrical insulation tape with a glass-cloth backing and a non-corrosive, flame-retardant, thermosetting silicone pressure-sensitive adhesive. The adhesive applies without heat or moisture preparation, while the glass-cloth construction provides a defined tape format for high-temperature electrical assembly. The tape is designed for continuous operation not exceeding 200 deg C under its UL listing and 180 deg C under its CSA listing. Its electrical and mechanical properties suit insulation, splicing, bundling, and coil-wrapping applications where a glass-cloth tape is specified.
Key features
- High-temperature electrical insulation: The tape is rated for continuous operation up to 200 deg C under UL and 180 deg C under CSA.
- Glass-cloth silicone construction: A 0.140 mm glass-cloth backing with thermosetting silicone adhesive provides a 0.178 mm insulation tape.
- Ready pressure-sensitive application: The adhesive applies without heat or moisture preparation for coil, transformer, and motor assembly.
Applications
It is used for coil, transformer, and motor insulation, lead anchoring, high-temperature electrical splicing, and bundling.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Other Properties
Mechanical Properties
Thermal Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Color | White | Visual | |
| Backing material | Glass cloth | As supplied | |
| Backing thickness | 0.140 | mm | Nominal |
| Total thickness | 0.178 +/- 0.025 | mm | ASTM D1000; 23 deg C |
| Adhesive | Thermosetting silicone | Pressure-sensitive | |
| Breaking strength | >= 263 | N/cm | Minimum; ASTM D1000; 23 deg C |
After-processing / final-state properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Dielectric breakdown | >= 2000 | V | Minimum; ASTM D1000; 23 deg C |
| Insulation resistance | >= 50 x 10^6 | ohm | Minimum; ASTM D1000 high-humidity method |
| Adhesion to steel | >= 3.3 | N/cm | Minimum; ASTM D1000; 23 deg C |
| UL continuous operating temperature | 200 | deg C | Do not exceed; UL listing |
| CSA continuous operating temperature | 180 | deg C | Do not exceed; CSA listing |