3M EC-2214

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

3M EC-2214

Main features

  • Premixed One Part Processing
  • Heat Cured Structural Bonding
  • Application Specific Grade Selection

Product Description

3M Scotch-Weld Epoxy Adhesive EC-2214 is a one-part, 100% solids epoxy paste that heat cures at a 121 deg C bondline temperature for structural bonding of metals, fiberglass-reinforced plastic, polyester, phenolic materials, and other high-temperature plastics. The EC-2214 family includes Regular, Hi-Density, Hi-Temp, and Hi-Temp New Formula grades. Regular is aluminum filled for general-purpose bonds, Hi-Density is deaerated for dense void-free bondlines, and the Hi-Temp grades target higher-temperature strength. The exact grade must be selected before cure and performance values are applied.

Key features

  • One Part Heat Cure System: The premixed paste removes a separate two-component mixing step.
  • Metal And High Temperature Plastic Bonding: The epoxy family supports compatible metals and reinforced polymer substrates.
  • Application Specific Grade Options: Regular, high-density, and high-temperature constructions address different bondline needs.

Applications

Heat-cured structural bonding of prepared metals, fiberglass-reinforced plastic, polyester, phenolic materials, and compatible high-temperature plastics.

Product Family

3M EC-2214

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Technical Specifications

No specifications available.

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers