LOCTITE ABLESTIK 8301 S1

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE ABLESTIK 8301S1

Main features

  • Snap cure
  • Hot die shear strength
  • Improved JEDEC performance

Product Description

LOCTITE ABLESTIK 8301 S1 is the exact same product as ABLESTIK 8301 but with 25um spacers.  This electrically conductive die attach adhesive is designed for high reliability package applications. It is a snap curable low stress epoxy hybrid with high reliability.

LOCTITE ABLESTIK 8301 S1 is used for a wide range of package sizes and can be used on PPF, Bare copper and silver substrates. It has been typically used and trusted for automotive sensor applications with great success.

Snap Cure

  • 7 zone Oven, 150 -240°C
  • Time: 60 seconds

Please check the TDS for additional details.

Product Family

ABLESTIK 8301 S1

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 55 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°CWork life @25°C
24 hours
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
2 °C
Thermal ConductivityThermal Conductivity
0.9 W/m.K
Electrical Properties
Volume ResistivityVolume Resistivity
0.0001 Ohms⋅cm
Chemical Properties
Moisture absorptionMoisture absorption
0.25 %
Physical Properties
Thixotropic indexThixotropic index
4.8
ViscosityViscosity
10,000 mPa.s

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers